CX-025493: Enhancing Yellowjacket for Modeling the Impact of Radiation and Stress on the Corrosion of Molten-Salt-Facing Structural Components-University of Florida

The University of Florida (UF) proposes to add the capability to the Yellowjacket code to model the impact of radiation and stress on the corrosion…

Office of NEPA Policy and Compliance

September 17, 2021
Estimated Read Time   min

The University of Florida (UF) proposes to add the capability to the Yellowjacket code to model the impact of radiation and stress on the corrosion of molten-salt-facing structural components.