CX-022591: Mitigating Stress Corrosion Cracking in Austenitic Stainless-steel Canister Welds Using Peening Techniques

The University of Nevada at Reno proposes to propose to develop mitigation of the possible initiation of pitting/stress corrosion cracking (SCC) in…

Office of NEPA Policy and Compliance

August 10, 2020
Estimated Read Time   min

The University of Nevada at Reno proposes to propose to develop mitigation of the possible initiation of pitting/stress corrosion cracking (SCC) in dry storage canisters austenitic stainless-steel welds by applying laser shock peening, shot peening and ultrasonic impact peening as well as indirect laser shock surface patterning methods (LSSP).