CX-018997: Cold Spray Repair and Mitigation of Stress Corrosion Cracks in Spent Nuclear Fuel Dry Storage Containers – Purdue University

Categorical Exclusion Determination

Office of NEPA Policy and Compliance

August 3, 2018
Estimated Read Time   min

Purdue University, in collaboration with Sandia National Laboratory and VRC Metal Systems, proposes to demonstrate cold spray repair and mitigation of chloride-induced stress corrosion cracking and pits in American Iron and Steel Institute 304 stainless steel dry storage canisters.